• Home
  • Download PDF
  • Order CD-ROM
  • Order in Print
Camshaft and Gear - Inspection (1-15)
Camshaft Lobe Edge Deterioration (Break- down) Criteria (1-17)

Interim High-Mobility Engineer Excavator Nsn 2420-66-148-7692
Page Navigation
  228    229    230    231    232  233  234    235    236    237    238  
img
TM 5-2420-230-24-2
Camshaft and Gear - Inspection (1-15)
Section 1 - Cylinder Block - Group 1
Page 1-30
B Series Shop Manual
Measure the bearing journals.
Journal Diameter
mm
in
53.962
MIN
2.1245
54.013
MAX
2.1265
Camshaft Lobe Pitting Reuse Criteria (1-16)
A single pit should not be greater than the area of a 2 mm
[.079 in] diameter circle.
Interconnection of pits is not allowable and is treated as
one pit.
The total pits, when added together, should not exceed a
circle of 6 mm [0.236 in].
L-233


Privacy Statement
Press Release
Contact

© Copyright Integrated Publishing, Inc.. All Rights Reserved.